40 Milliounen | Eenheet | Gm70 | Gm70a | Gm70d | ||||
Décker | μM | 30 | 36 | 30 | 36 | 30 | 36 | |
Tensil Stäerkt | MD | MPa MPa | 2266 | 218. | 240 | 2288 | 213 | 190 Joer |
TD | MPa MPa | 2522 | 262 | 269 | 251 | 246. Mee 246 | 2277 | |
Erlong | MD | % | 134 | 146 | 148 | 145 | 1322 | 147 |
TD | % | 111 | 1022 | 113 | 115 | 109 | 104 | |
Kréien (150 ℃ / 30min) | MD | % | 1.19 | 1.23 | 1.26 | 1.21 | 1.11 | 1.05 |
TD | % | 0,11 | 0,344 | 0,13 | 0.21 | 0,08 | 0,2 | |
Seranzwanz | % | 89.8 | 89.6 | 90.2 | 90.3 | 90.1.1 | 90,0 | |
Echegner sinn | % | 3.23 | 5.42 | 3.10 | 3.37 | 3.38 | 4.29 | |
Rauhness | Ra | nm | 22 | 24 | 34 | 32 | 15 | 18 |
Rz | nm | 219. | 2399 | 318 | 2955 | 118 | 143 | |
RMappi | nm | 302 | 334 | 461 | 4588 | 165 | 189 |